Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

reinforced concrete buttress design

Status
Not open for further replies.

smulmi

Structural
Joined
Nov 3, 2011
Messages
16
Location
US
Hi all,

I am looking at designing a RC buttresses to reinforce an existing rubble masonry wall. I sized the buttress walls (8' on centers) to resist the overturning and sliding forces. I had to anchor the buttresses to the soil (rock) below. My question is how do I design the rebars for the buttresses?

Any suggestions and/or references are welcome. Thanks in advance.
 
Most folks would design them like a conventional shear wall. One design for all, and do not vary it unnecessarily - this is a matter of economy. You can use strut and tie, but the design needs to be uniform and/or uncomplicated to minimize construction problems and cost. Steel reinforcement is not expensive compared to the labor required to construct a complicated design.

That said, relatively short buttresses may provide sufficiently for shear using Vc alone. The reinforcement would then be needed to meet minimums (in both directions - use the ACI 350 minimum to reduce crack width) and to provide tension tie to the foundation.
 
look up counterforts. I would think the reinforcing would be near the concrete face touching the rubble wall (assuming an exterior buttress on an arched building or a retaining wall - not sure what the rubble wall is for).
 