relentlessratt
Mechanical
i am starting a new house project and would like some advise with regards to the design of a concrete beam.Tthe detail for the Reinforced concrete beam which sits above the garage is described below:
Beam size: 12" wide x 20" Depth
Top Reinforcement: 6x5/8" Rebar at 1/3 span to the ends of the beam. the Center 1/3 is reinforced with 3x5/8" rebar.
Bottom reinforcement: 6x5/8" Rebar for the center 1/3 span. 1/3 of the span on the ends is reinforced with 3x5/8" rebar.
The contractor has indicated that the quantity of of reinforcement may create an issue when pouring concrete and may cause voids. he has suggested that the rebar diameter be changed from 5/8" to 1" and reduce the quantity of rebar to 6 pieces (3 to the top and 3 below).
can someone with construction experience/knowledge provide some advise on this?
Beam size: 12" wide x 20" Depth
Top Reinforcement: 6x5/8" Rebar at 1/3 span to the ends of the beam. the Center 1/3 is reinforced with 3x5/8" rebar.
Bottom reinforcement: 6x5/8" Rebar for the center 1/3 span. 1/3 of the span on the ends is reinforced with 3x5/8" rebar.
The contractor has indicated that the quantity of of reinforcement may create an issue when pouring concrete and may cause voids. he has suggested that the rebar diameter be changed from 5/8" to 1" and reduce the quantity of rebar to 6 pieces (3 to the top and 3 below).
can someone with construction experience/knowledge provide some advise on this?