Oct 30, 2016 #1 purode333 Mechanical Joined Sep 16, 2016 Messages 58 Location NG Dear sir, To weld the cran rail of CR 100, which electrode we have to use. We want to implement the SMAW process instead of thermit welding. Pls suggest best and commonly use electrode. Regards Prasad
Dear sir, To weld the cran rail of CR 100, which electrode we have to use. We want to implement the SMAW process instead of thermit welding. Pls suggest best and commonly use electrode. Regards Prasad
Nov 4, 2016 #2 Mr168 Materials Joined Aug 5, 2008 Messages 731 Location US I recommend you look into Metrode Railrod and the associated fabrication practices they prescribe. Upvote 0 Downvote
Nov 12, 2016 Thread starter #3 purode333 Mechanical Joined Sep 16, 2016 Messages 58 Location NG Dear all from eng-tips, Pls suggest me best and commonly use electrode. hope so. Regards Prasad Upvote 0 Downvote
Nov 13, 2016 #4 GenB Mechanical Joined Oct 24, 2003 Messages 1,362 Location US I thi k that you need expert Eng advise, else that loco will derail. General Blr. CA,USA Upvote 0 Downvote