I'm looking for a reference to substantiate a braze repair. I'm brazing an Inconel 625 doubler to an Inconel 625 part using a nickel foil braze per AMS 4777. MMPDS-01 only has shear allowable for copper and silver brazing both of which it gives as 15 ksi. I found the article "Design properties of brazed joints for high temperature applications" by R L Peaslee and W M Boam which shows graphically that nicrobraz brazing has better qualites then silver or copper brazing.
I want to use the 15 ksi figure, which would give me a large margin of saftey, but I can't find any specific reference to substantiate that number. Does the community have any references I can use, or would referencing this article be enough? The article does not deal specifically with the materials I am using but s 590 (ams 5770) and nicrobraz 125.
Thanks,
-Kirby
I want to use the 15 ksi figure, which would give me a large margin of saftey, but I can't find any specific reference to substantiate that number. Does the community have any references I can use, or would referencing this article be enough? The article does not deal specifically with the materials I am using but s 590 (ams 5770) and nicrobraz 125.
Thanks,
-Kirby