LiftDivergence

Aerospace
Joined
Jan 15, 2014
Messages
278
Location
US
Hi all,

A few months ago I saw an post to the "Aircraft Structures" group on LinkedIn. I'm not going to link to to the post because I don't want to link to external sites in the forum. But this is a public group on LinkedIn with ~27,000 members where various aircraft structures are discussed, usually structural repairs.

The post in question was showing a repair for an aft fuselage skin belt loader impact on a circumferential splice. A large area of the skin was pretty severely dented and buckled in. They trimmed out a large area both skin panels across the splice. I have attached some pictures of the trimout and also the completed repair (external and internal).

What immediately struck me about the repair was their choice to design it as a "split patch". Effectively, one doubler for each skin panel with no continuity between them (other than the replaced production internal splice strap).

In my experience, I would have expected a repair for this damage would either have a continuous doubler over the splice, or a tripler layer over the split doublers. This comes both from familiarity with SRM repairs for several different makes/models of aircraft where a trimout is made on a skin splice, and from analysis experience of reinforcements spanning damage across splices.

There is some discussion on the post pointing this out. However, the individual who posted the repair seemed adamant that this was correct.

I'm curious what people think of the pros & cons of this design. I have my opinion of course, but I'm curious what other peoples experiences are.

1736374979000.jpg

1736374973125.jpg

1736374980757.jpg
 
Opinions are like ...

If I had a to patch over a splice strap, I would probably (depending on specifics blah, blah, blah ...) combine the splice strap into the repair dbr ...

cut out the damage (or cancer as I'll often call it),
rebuild frames and stringers,
then add a large repair dblr over the cut-out and splice into the external splice strap (and this could be simple butt joint or a small splice strap).

To say a particular repair is "right" (which implies all others are "wrong") is IMHO pedantic ... so long as the repair considers all the necessary issues (particularly DTA) then all should be "good". Sure some repairs will be lighter than others, but is that Really significant ? Sure, it can be, but often isn't. Sure there are badly designed repairs ... because they haven't considered some aspect or another (like super heavy repair doublers, attracting load, making the "repair" worse).

We had an operator do a repair on something we'd built (many years before) under their own paperwork, so not my problem. But I looked at it and was pretty horrified ... they had rebuilt the OEM structure (that had cracked) precisely without thinking/asking and it was pretty "wimpy" ('cause that suited the OEM's environment). Making the repair match exactly the OEM structure (like splitting the repair dblr into two pieces to match the OEM skin panels) is not IMHO the right thing to do (by default).
 
Is this correct- that the original skin had a discontinuity over the middle of the internal splice strap and that the repair has the same discontinuity over the same section internal splice strap replacement?

Is it possible the patches were removed from out-of-service aircraft rather than having custom formed replacements?

A single piece would also be stiffer across the splice than the surrounding material, though I suppose the doublers already are.

It doesn't look like there's any fundamental problem with the patch.
 
I can see some "hand wringing" over the single repair patch creating a different loadpath over the skin splice, and how some may want to repeat the fuselage testing to account for this. But I'd've thought that this additional loadpath over the fuselage splice makes it more effective (and I hear "exactly, it'll attract more load than the OEM design ...") but I see the splice joint as trying to make the edges of the fuselage panels "disappear" and anything that makes this better is good (if it is fully analyzed ... "so how do you analyze for the additional load ?").

I would've made it a single repair dblr and rested very well (I would've been more worried about some unnoticed damage from the original incident ... maybe annual visual inspections of the surrounds to verify).
 
10 points to the baggage handler for missing the frames :)
 
I have less experience with metal fuselages than composite structures, but I disagree,
I would repair as shown in the photos; then the bolted joint load transfer will be very similar to baseline structure, and there will not be any stress concentrations in the doubler where it spans the splices; particularly when the doubler is not a simple rectangle but has corners at the splice.
And definitely if this is a composite fuselage, do not put a doubler spanning over a body splice location.
 
Good discussion points. I agree the concept of "right" and "wrong" is only relevant insomuch as the repair needs structural substantiation which is approved by an authorized representative, which we have to assume it was.

However, I do feel that there are objectively relatively better and worse repair practices. And my main concern is that the linkedin forum is highly active with a lot of M&Ps, etc. looking at this.

Every repair from a structural repair manual I am familiar with (Boeing, MD, Airbus, Embraer, etc) were a trimout of skin common to a splice takes place - the reinforcing material spans OVER the splice.

And not just that - from an analysis perspective, the skin and circumferential splice plate are biaxially loaded. Yes, the skin panels normally terminate at this location. But the repair is affecting the total stackup and the joint load transfer at the splice in both directions. The doublers are hardpointing the splice plate circumferentially and also adding stiffness and outer row R/P longitudinally. The splice plate is getting "hit harder" than it is in production. Effectively, you are asking it to function normally and also act as part of a new repair stackup.

I would WANT to be creating a new load path over the splice which is handled as part of the analysis. I think it's important to consider not just the skin, but how adding a new layer to the OML will affect all of the faying substructure. Which is IMO why any SRM repair addressing this type of damage has a layer bridging the splice.

But all perspectives are appreciated.
 
Has nobody noticed the existing skin joint at the longeron? Look carefully at the upper photo, left skin panels. There's an upper and a lower skin panel there. That complicates the picture, for me. We aren't dealing with a single skin joint.

The damage removals are not aligned with each other. The repair on either side was done with an external doubler and internal filler to ensure the joints and panels line up properly. The internal fillers are probably not continuous across the frame joint, and good thing, IMO, considering the change in WaterLine of the damage area in the two panels. That's a shift of 4 to 5 inches (10 to 13 cm). If the filler were continuous through that, then there would be a weird "shear" in the filler panel that could do odd things. Therefore the internal filler must be divided at the frame.

OK, now that I've figured that out, do I still want the doubler to be continuous over the joint? Why? The joint already has enough fasteners for a complete load transfer into the tear-strap.

So there's 3 reasons for you to question your intuition. Nothing wrong with intuition - just know what it's based upon so you can use it at the right time.

If you were to review the "standard" SRM repairs and pick ones that cross a skin joint, are you sure they aren't always assuming the damage is located in a single area?

A different way to ask a similar question: How far offset do the two skin damage areas need to be from the same waterline, before you WOULD consider making the repair doubler into two panels?
 
Yes, and that is actually, in my opinion, another issue with the repair. Examining the photo which is an external view looking in - as you say on the (presumably) FWD skin panel there is a longitudinal splice as well. But it is not a typical lap splice, there appears to be an internal longitudinal splice strap.

The damage on the FWD panel was removed by trimming out a segment of skin all the way up to the splice.

In the pictures I had posted, I didn't include the original damage on the LinkedIn post, but the denting from the loader strike went all the way up to this splice area.

So standard practice IMO, if you are removing damage skin common to a splice, the reinforcement needs to extend over the splice, normally at least 3 rows for the full stackup, and 4 if you are using a doubler/tripler combo.

This repair installs a repair layer which ends at the nominal splice location, picking up the same holes.

If it were my design I would have extended the FWD panel repair up and over that splice.

Sparweb, to answer your question about the continuity of the filler, I have attached another picture of the interior which shows that it is not divided. It appears continuous over the splice. I agree with you on the filler, I feel that should be two parts which terminate on the circumferential splice plate, and then, as I wrote above, the external repair should be continuous across the splice, or at least have a tripler which is.

Lots of details with this repair seem "off" if you really look at it. Which is why I brought it up.

A different way to ask a similar question: How far offset do the two skin damage areas need to be from the same waterline, before you WOULD consider making the repair doubler into two panels?
I would review some data / studies of stress effect for reinforcements in close proximity (like RAPID). I would want to ensure the stress interaction factors /effects were minimal or negligible before keeping them separate. In this scenario I think combining the damage on each panel into a single repair is the right way to go.

1736374966960.jpg 1736374979339.jpg
 