reference Material - Repairs of Composite Aircraft Structures

Status
Not open for further replies.

mrbliaison

Aerospace
Apr 7, 2003
6
Can anyone recommend some reference material in regards to repairs of composite aircraft structures within a MRB liaison environment? Thanks.
 
Replies continue below

Recommended for you

Can be more precise you about the type of repair and material?
 
Check the aircraft SRM, Chap 51-70 usually contains all composite repairs.
 
The book "Care and Repair of Advanced Composites" Armstrong and Barrett

SAE has several recommended practice publications (ARP's) for composite repair for sale at
 