0707
Petroleum
- Jun 25, 2001
- 3,433
Is it correct to rebuild a 5meter 17-4 PH material, fatigue broken shaft thought a SS 410 welded sleeve ring? What would be the filler material for joining 17-4 PH with SS TP 410? What kind of PWHT would be required? What would be the alternatives to such repairing?
Thank you