OUR MIX DESIGN HAS A SLUMP AT SITE 125 mm +/- 25mm with super plasticizer but usually, concrete arrived at site is less than the minimum or more than the maximum specified slump in the design mix. Is it right the QC inspector can reject the concrete?
Example Case: 1 truckmixer has slump at site 40mm only while the 2nd trucmixer has slump at site 240mm. Design mix is 28 MPa with super plasticizer; slump at site 125 +/- 25mm. These two trucload of concrete were rejected. Is it right for the inspector to reject the concrete?Pleae any expert on this may give his opinion is highly appreciated. Thanks a lot...
Example Case: 1 truckmixer has slump at site 40mm only while the 2nd trucmixer has slump at site 240mm. Design mix is 28 MPa with super plasticizer; slump at site 125 +/- 25mm. These two trucload of concrete were rejected. Is it right for the inspector to reject the concrete?Pleae any expert on this may give his opinion is highly appreciated. Thanks a lot...