Sep 24, 2019 #1 TheEverest Mechanical Joined Aug 28, 2019 Messages 72 Location NP Dear all. According to table UCS-57, the nominal thickness above which full-radiography is needed is given as1.25 inch for P.no. 1 and Gr.1,2,3 material. Does this include the thickness 1.25 inch as well?
Dear all. According to table UCS-57, the nominal thickness above which full-radiography is needed is given as1.25 inch for P.no. 1 and Gr.1,2,3 material. Does this include the thickness 1.25 inch as well?
Sep 24, 2019 #2 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,120 Location NL No. See Interpration VIII-81-102 if semantics is an issue in the translation. Upvote 0 Downvote
Sep 24, 2019 Thread starter #3 TheEverest Mechanical Joined Aug 28, 2019 Messages 72 Location NP Do you mean that full radiography is for only nominal thickness above 1.25 inch and not for 1.25 inch? Upvote 0 Downvote
Do you mean that full radiography is for only nominal thickness above 1.25 inch and not for 1.25 inch?
Sep 24, 2019 #4 david339933 Industrial Joined Jun 15, 2011 Messages 1,204 Location CA Correct. Upvote 0 Downvote
Sep 25, 2019 Thread starter #5 TheEverest Mechanical Joined Aug 28, 2019 Messages 72 Location NP Thank you David!! Upvote 0 Downvote