Can you help me:
If ASME IX said:
QW-203 LIMITS OF QUALIFIED POSITIONS FOR PROCEDURES Unless specifically required otherwise by the welding variables (QW-250), a qualification in any position qualifies the procedure for all positions
Then Why piping are tested to qualify wps position 6g , if a 1G position is enough
Thanks
JATE
If ASME IX said:
QW-203 LIMITS OF QUALIFIED POSITIONS FOR PROCEDURES Unless specifically required otherwise by the welding variables (QW-250), a qualification in any position qualifies the procedure for all positions
Then Why piping are tested to qualify wps position 6g , if a 1G position is enough
Thanks
JATE