Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

QW-321.2 Immediate Retest Using Mechanical Testing

Status
Not open for further replies.

sftyvlv1

Mechanical
Oct 25, 2018
48
How would I apply this paragraph to a 6g pipe test?
Would I have the welder weld out a new test or root an entire test, fill and cap the section that failed?
What should happen?
 
Replies continue below

Recommended for you

The welder must complete two full 6G test coupons and both must pass mechanical testing.
 