How would I apply this paragraph to a 6g pipe test?
Would I have the welder weld out a new test or root an entire test, fill and cap the section that failed?
What should happen?
 
The welder must complete two full 6G test coupons and both must pass mechanical testing.
 
Thanks, much appreciated.
 