According to Qw-153 (C) ASME Sec IX specimens shall have a tensile strength more than minimum specified tensile strength of the weld metal when the applicable Section provides for the use of weld metal having lower room temperature strength than the base metal.
Now, please tell me about “applicable Section”. In which Section, “use of weld metal having lower strength” is provided and why?
tanks
Regards
H.Mirhosseini