KENAT
Mechanical
- Jun 12, 2006
- 18,387
I posted thread1103-172691 asking about standard US commercial weld notes but didn't get a complete answer. Anyone here have some ideas. The below is what I had in the UK (they may be a little out of date as the specs kept changing)
1. Weld symbols comply with BS EN 22553.
Steel
2. Welding to be in accordance with BS EN 1011 Parts 1 & 2 using MIG or TIG process using filler rod to BS EN 440.
Stainless
2. Welding to be in accordance with BS EN 1011 Parts 1 & 3 using MIG or TIG process using filler rod to BS EN 440.
Alluminum
2. Welding to be in accordance with BS EN 1011 Parts 1 & 4 rods or filler to BS2901
For note 1 I’m happy that referencing AWS 2.4 covers this, actually since we reference Y14.100 on our standard notes I arguably don’t need to call our AWS 2.4 specifically.
However, guidance on what to put for note 2 would be appreciated.
1. Weld symbols comply with BS EN 22553.
Steel
2. Welding to be in accordance with BS EN 1011 Parts 1 & 2 using MIG or TIG process using filler rod to BS EN 440.
Stainless
2. Welding to be in accordance with BS EN 1011 Parts 1 & 3 using MIG or TIG process using filler rod to BS EN 440.
Alluminum
2. Welding to be in accordance with BS EN 1011 Parts 1 & 4 rods or filler to BS2901
For note 1 I’m happy that referencing AWS 2.4 covers this, actually since we reference Y14.100 on our standard notes I arguably don’t need to call our AWS 2.4 specifically.
However, guidance on what to put for note 2 would be appreciated.