Jul 10, 2001 #1 Dragon Industrial Joined Dec 21, 2000 Messages 8 Location IE Heh people. Anyone got any ideas as to what PBAX Nylon is??? What do the letters PBAX stand for? All help greatly appreciated. Dragon.
Heh people. Anyone got any ideas as to what PBAX Nylon is??? What do the letters PBAX stand for? All help greatly appreciated. Dragon.
Jul 10, 2001 1 #2 plasticbob69 Materials Joined Jan 4, 2001 Messages 8 Location US Dragob, PEBAX is the tradename of Elf Atochem's PEBA (polyether block amide) You can get more info at their site. Best regards, Upvote 0 Downvote
Dragob, PEBAX is the tradename of Elf Atochem's PEBA (polyether block amide) You can get more info at their site. Best regards,