newweldeng09
Mechanical
I am joining 4130 to a P1, Gr. 2 carbon steel. Impact testing is required. The 4130 base metal was impact tested to meet 37/25 ft-lbs. The carbon steel was impact tested to meet 18/12 ft-lbs. Why do I have to impact test the 4130 HAZ to meet 37/25 ft-lbs. and the carbon steel HAZ to meet 18/12 ft-lbs. as required by UG-84(g)(5)? Why can't I qualify the procedure using the lower energy requirement as a minimum?