Oct 20, 2015 #1 dho Mechanical Joined May 19, 2006 Messages 255 Location US what is the mechanical properties of 303 stainless steel listed under QQ-S-763C? thanks.
Oct 21, 2015 #2 israelkk Aerospace Joined Dec 30, 2002 Messages 2,280 Location IL To my best knowledge QQ-S-763 doesn't list 303 which is a free cutting version of 302. 303 is covered by ASTM A 581. Upvote 0 Downvote
To my best knowledge QQ-S-763 doesn't list 303 which is a free cutting version of 302. 303 is covered by ASTM A 581.
Oct 21, 2015 Thread starter #3 dho Mechanical Joined May 19, 2006 Messages 255 Location US 303 was listed in qq-s-763 revision C and older. not in rev D and later. C is no longer available (free) at government site. Upvote 0 Downvote
303 was listed in qq-s-763 revision C and older. not in rev D and later. C is no longer available (free) at government site.
Oct 21, 2015 #4 israelkk Aerospace Joined Dec 30, 2002 Messages 2,280 Location IL Yes you are correct. Here is a note I have found in QQ-S-763E. 6.4 Classes 303, 303Se, 416, 416Se, 430F and 430F Se under QQ-S-763C should be purchased to ASTM A 484 and ASTM A 582 or ASTM A 555 and 581. Upvote 0 Downvote
Yes you are correct. Here is a note I have found in QQ-S-763E. 6.4 Classes 303, 303Se, 416, 416Se, 430F and 430F Se under QQ-S-763C should be purchased to ASTM A 484 and ASTM A 582 or ASTM A 555 and 581.