Based on the e-mail reply that I received from Battel Columbus "The equation included with each MMPDS S/N curve is the typical regression line, 50% survival. And, the 97.7% survival probability can be computed, by subtracting 2.0 x the standard error of the estimate from the typical line."
Thanks,
A.