Nov 4, 2014 #1 sathikn87 Mechanical Joined Oct 30, 2014 Messages 12 Location SA Hii there, Which code in ASME sec viii governs the requirement of PWHT is mandatory or not? Thanks
Nov 5, 2014 1 #2 jwhit Materials Joined Apr 3, 2012 Messages 202 Location US Read UW, UCS, UHA and any other sections that might pertain to your material. Upvote 0 Downvote
Nov 13, 2014 #3 Adeeba Mechanical Joined Nov 13, 2014 Messages 6 Location PK Read UCS 56 Upvote 0 Downvote
Nov 21, 2014 1 #4 Kurniatullah Mechanical Joined Oct 20, 2012 Messages 16 Location ID Dear Jithin214 for your reference Procedure PWHT ==> UW40 Procedure Local PWHT ===> UW40 and refer to WRC BULLETIN 452_JUNE-2000 Requirement PWHT for Carbon Steel ==> UCS 56 Upvote 0 Downvote
Dear Jithin214 for your reference Procedure PWHT ==> UW40 Procedure Local PWHT ===> UW40 and refer to WRC BULLETIN 452_JUNE-2000 Requirement PWHT for Carbon Steel ==> UCS 56