Hii there,
Which code in ASME sec viii governs the requirement of PWHT is mandatory or not?
Thanks
 
Replies continue below

Recommended for you

Read UW, UCS, UHA and any other sections that might pertain to your material.
 
Dear Jithin214

for your reference

Procedure PWHT ==> UW40
Procedure Local PWHT ===> UW40 and refer to WRC BULLETIN 452_JUNE-2000
Requirement PWHT for Carbon Steel ==> UCS 56
 