I need some help regarding the table K323.3.1(impact testing requirements) of ASME B31.3 (2012):
According to that table it is required to perform PRODUCTION TEST (impact test) for each WPS / type of electrode / each range: 1/2T to T+6mm(1/4").
If impact test are performed as part of WPS qualification, still necessary to perform production tests on fabrication welds?
Best regards.
According to that table it is required to perform PRODUCTION TEST (impact test) for each WPS / type of electrode / each range: 1/2T to T+6mm(1/4").
If impact test are performed as part of WPS qualification, still necessary to perform production tests on fabrication welds?