My company has been asked to fabricate some pressure vessels,
The material specified is sa516 70 the lead time on this plate is too long, Where SA/AS1548 7 490n is readily
available (vessel 40mm tk gas scrubber), Would this be an acceptable substitute to verify the drawings to AS1210
class 1.Currently drawings are ASME VIII(very similar codes).The vessels are for use in australia hence reverification to AS1210
7490n is listed on bluescope steels web site as xlerplate.
Any help would be greatly appreciated
The material specified is sa516 70 the lead time on this plate is too long, Where SA/AS1548 7 490n is readily
available (vessel 40mm tk gas scrubber), Would this be an acceptable substitute to verify the drawings to AS1210
class 1.Currently drawings are ASME VIII(very similar codes).The vessels are for use in australia hence reverification to AS1210
7490n is listed on bluescope steels web site as xlerplate.
Any help would be greatly appreciated