Does anybody know what would be the equivalent ASME spec?
 
Replies continue below

Recommended for you

Hi,
According to the German Stahlschlussel, the possible equivalents are:
A-516 Gr. 65 ; 55
A-515 Gr. 65 ; 55
A-414 Gr. C
A-442 Gr. 55
 