Hi there
I’d kindly need some help for following topic.
I’d need to verify a pressure vessel for a design temperature higher than material creep temperature,ex 410F.
Question 1)
Do you think it is feasible ?
My understanding is that this is possible, but a specific number of hours, or cycles, will be determined.
After that the vessel will break.
Please, is this correct ?
Should it be possible following would be my procedure, but, if I am wrong, I would be extremely grateful if somebody could correct me.
Following would be my steps
1) Calculate longitudinal stress as
Sigma = P*D/(2*t)
2) Take the Woehler diagram for copper
3) Apply correction factors for thickness and temperature
4) Individuate which is the total number of cycles that Woehler diagram will give me for the calculated sigma (1&3) utilizing Woehler diagram
Questions
1) Is this method correct according to your knowledge & experience ?
2) Could you please tell me where to find the Wohler curve for copper ?
3) Should not, which would be the method you’d apply ?
4) Is there codified method ( ex ASME, or German AD ?) to solve this topic
Thanks in advance for your help
I’d kindly need some help for following topic.
I’d need to verify a pressure vessel for a design temperature higher than material creep temperature,ex 410F.
Question 1)
Do you think it is feasible ?
My understanding is that this is possible, but a specific number of hours, or cycles, will be determined.
After that the vessel will break.
Please, is this correct ?
Should it be possible following would be my procedure, but, if I am wrong, I would be extremely grateful if somebody could correct me.
Following would be my steps
1) Calculate longitudinal stress as
Sigma = P*D/(2*t)
2) Take the Woehler diagram for copper
3) Apply correction factors for thickness and temperature
4) Individuate which is the total number of cycles that Woehler diagram will give me for the calculated sigma (1&3) utilizing Woehler diagram
Questions
1) Is this method correct according to your knowledge & experience ?
2) Could you please tell me where to find the Wohler curve for copper ?
3) Should not, which would be the method you’d apply ?
4) Is there codified method ( ex ASME, or German AD ?) to solve this topic
Thanks in advance for your help