Can you advise if Pressure test requirments of tie in welds which shall be subject to UT & MPI. the manifold has been pre fabricatied and all welds have been x-rayed and pressure tested to 1.5 desgin pressure.

Question: is system subject to pressure test 1.5x desgin pressure or 1.1 ?
 
Replies continue below

Recommended for you

i thought the test pressure was changed to 1.3X
 
Eck75,

Pneumatic pressure test???
For pneumatic test you may consider 1.1 x design pressure...
 
No, not for tie in welds. As long as a volumetric examination of the tie in welds is completed, there should be no need for a pressure test.
 