Does anyone out there know of any software to predict case depth, etc for steels when gas carburizing. I found something called "Carburizing!", but it only seems to be available as a demo.

Thanks
 
You may see "GAS CARBURIZING, AMERICAN SOCIETY FOR METALS, 1964 " or " 1977, American Society for Metals Metals Park, Ohio - Carburizing and carbonitriding ".
the later has figures which give you depth of case vs. time and temprature of carburizing.
 