On the incline panel, if the over-hang is constant at 2m and the height varies from 0.5m to 3m it would seem that these panel are twisted which is going to be very hard to cast. It would take a special adjustable bed that could be twisted as required and I have never seen or heard of anything like that.
From a casting standpoint, it would be far better to pick an incline angle for all panels. If that cannot be done, maybe the incline panel should be made from something that can be twisted to fit rather than using concrete which must be cast to fit.