Good morning and excuse me for my English
the question is:
I need to qualify (in accordance with ASME code sec IX) the welding procedure of a pipe A333 Gr6 with a pipe A335 P11 (Cr-Mo-Si).
The job temperature is -15°C. I shall do Impact test in Weld Metal - Base Metal - HZA, to -20°C.
It is necessary to do Impact test on Base metal on pipe A335 P11? The pipe material certificate is tested at +20°C.
Many thanks
Regards
jean71
the question is:
I need to qualify (in accordance with ASME code sec IX) the welding procedure of a pipe A333 Gr6 with a pipe A335 P11 (Cr-Mo-Si).
The job temperature is -15°C. I shall do Impact test in Weld Metal - Base Metal - HZA, to -20°C.
It is necessary to do Impact test on Base metal on pipe A335 P11? The pipe material certificate is tested at +20°C.
Many thanks
Regards
jean71