I'd want to get some advice from a TIG aluminum welding expert.
Get help with WPS, PQR documentation, and welder exams.
As you can see, my company recently purchased an old welding machine for this purpose.
We need to fabrication piping and repair silo with referring Code ASME IX

118146_zqxllv.jpg
118143_ww68x5.jpg

118145_tob2e0.jpg
118147_mainmm.jpg

118148_q57h9n.jpg
118144_s7nqvf.jpg

118149_z0mgsv.jpg
 
The simplest response I can give to a three week discussion is; wait for it: clean the base metal, clean the filler metal, wear chrome tanned gloves (not oil tanned) and don't use abrasives that utilize aluminum oxide "grit".

Best regards - Al
 