Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Please anyone have any suggestions for dealing with or repairing pipe corrosion?

Status
Not open for further replies.

inaro

Civil/Environmental
Joined
Nov 9, 2020
Messages
1
Location
ID
In this case my hydrant pipe was exposed by corrosion, i thought it was caused by the humidity and water droplets
Please anyone have any suggestions for dealing with or repairing pipe corrosion?
thank you for any suggestions

image_2021-03-09_084123_rldgal.png
 
There are a few products here: Link A number of other suppliers are available. Google "composite pipe wrap repair"

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Contact your local Belzona rep if your pockets are deep enough.
 
Belzona may be a solution there are also tape fiber glass resins and also some epoxy linners.

regards

luis
 
First determine the severity of corrosion. If its superficial as it appears in the photo, remove surface contamination and recoat with a more appropriate coating than the one currently used.
 