I have been provided of a WPS and its respective supporting PQR. The qualified BM thickness range is shown in the WPS as 3/16" - 2" and Pipe 6" - Unlimited. PQR is showing test coupon of 1".
Does plate test coupon qualifiy a WPS also for pipe? I went through the code and I couldn't find anything that support this.
Does the code address qualifications based on thickness and type of joint, regardless if it is either pipe, or plate? If it does, where this 6" - unlimited range came from?
Kind regards,
Cesar
I have been provided of a WPS and its respective supporting PQR. The qualified BM thickness range is shown in the WPS as 3/16" - 2" and Pipe 6" - Unlimited. PQR is showing test coupon of 1".
Does plate test coupon qualifiy a WPS also for pipe? I went through the code and I couldn't find anything that support this.
Does the code address qualifications based on thickness and type of joint, regardless if it is either pipe, or plate? If it does, where this 6" - unlimited range came from?