Plastic Fuel Filler Neck Material:Gasoline/Diesel

Status
Not open for further replies.

AbiIndia

Automotive
Sep 4, 2003
1
Hi!
I am trying to find the material options available fuel filler neck for (i) Gasoline and (ii)Diesel applications.
PP,PA6,PA6+GF,PA66, HDPE, PA6+EPDM. I am confused. please help.

Regards
Abhilash
Pune, India
 
Replies continue below

Recommended for you

PE and PP will let gasoline and diesel through and soften. Of the choices PA 6 or PA 6,6 look best due to good mechanicals and oil (petroleum) resistance.

Chris DeArmitt PhD
President - Phantom Plastics LLC

Consulting, ideas and training on plastic materials
 
What are the plastic gas cans made from? I've always thought those were HDPE?