WE ARE FACING AN ISSUE OF CRACKING OF PLASTIC CAPS FITTED ON GLASS BOTTLES AFTER 7-10 DAS
 
Much more information required.
Cap screwed on too tight?

(Your caps lock button appears to be stuck on, btw)