Jun 22, 2023 #1 Xabi33 Automotive Joined Jul 26, 2020 Messages 4 Location SE Hi could someone share any good articles or insights on how the electrical resistivity of common thermoplastics (PP, PET, PC, etc.) changes when they melt?
Hi could someone share any good articles or insights on how the electrical resistivity of common thermoplastics (PP, PET, PC, etc.) changes when they melt?
Jun 22, 2023 1 #2 btrueblood Mechanical Joined May 26, 2004 Messages 10,034 Location US Generally it will go down - electron mobility increasing with temperature, etc. https://www.researchgate.net/figure...for-some-polymer-dielectrics-1_fig1_361653704 Upvote 0 Downvote
Generally it will go down - electron mobility increasing with temperature, etc. https://www.researchgate.net/figure...for-some-polymer-dielectrics-1_fig1_361653704
Jun 22, 2023 1 #3 Pud Mechanical Joined Mar 26, 2003 Messages 2,713 Location GB I would guess PVC would drop significantly as it degrades at melt temperatures with HCl as a byproduct. Politicians like to panic, they need activity. It is their substitute for achievement. Upvote 0 Downvote
I would guess PVC would drop significantly as it degrades at melt temperatures with HCl as a byproduct. Politicians like to panic, they need activity. It is their substitute for achievement.