Can anyone suggest about "How to find temperature rise during severe plastic deformation of a metal" say during torsion or any other deformation process ?
 
Replies continue below

Recommended for you

The area under the stress strain curve is an energy per unit volume. If you assume a perfectly plastic material and uniform deformation,

q = [σ][ε]pV

Also if it is adiabatic

q = mcp[Δ]T

If all the energy input is dissipate as heat

[Δ]T=[σ][ε]p/([ρ]cp)

If you have a less simple case, the idea is the same but it takes a little more work. Of course, as always watch the units.


 