Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Click mechanism on rotating plastic part

Status
Not open for further replies.

AriRnD

Mechanical
Joined
Jan 9, 2025
Messages
5
Hello, I am a newly hired mechanical R&D staff. Currently, I am working on designing a component for a medical device, and I am encountering an issue with one of the parts.

Below is the image of the sub-assembly component I am working on. The component can rotate from 0 to 90 degrees (The first image is when 0 degrees condition, second one is on 90 degree, and the third image is front view of the component), and at both the 0 and 90-degree positions, it is expected to have a click mechanism to secure these angles without adding additional components (such as springs, etc.). Do you have any suggestions or references for the design of this mechanism?

Screenshot 2025-01-09 152001.pngScreenshot 2025-01-09 152052.pngScreenshot 2025-01-09 152032.png
 
Last edited:
A full radius with notches at the stopping points is typically used (blue part) with a spring and round-end bullet in the red part.

This is the lowest cost, reliable method.

I suppose you could replace the spring and bullet with a zig-zag of plastic feature that is molded as part of the red part. If the red part is acetal (Delrin(R)) that would help. It will be tougher to adjust the feel than using a spring as to tweak it requires a mold change.

Look up compliant mechanism design.
 
- How many rotation cycles do you expect this assembly to see over it's life?
- Will the mechanism have to resist any external forces, or just the weight of the components?
- Is plastic debris from repeated use a contamination concern in a medical environment?
 
A full radius with notches at the stopping points is typically used (blue part) with a spring and round-end bullet in the red part.

This is the lowest cost, reliable method.

I suppose you could replace the spring and bullet with a zig-zag of plastic feature that is molded as part of the red part. If the red part is acetal (Delrin(R)) that would help. It will be tougher to adjust the feel than using a spring as to tweak it requires a mold change.

Look up compliant mechanism design.
Is the spring and bullet mean is ball plunger like this?
Screenshot 2025-01-18 080819.png

If all parts in the design are made using 3D resin printing, would it be reliable to use a zig-zag plastic feature for production?
After studying, I found that using a click mechanism with resin material is prone to cracking. Is this statement correct?
 
Last edited:
- How many rotation cycles do you expect this assembly to see over it's life?
- Will the mechanism have to resist any external forces, or just the weight of the components?
- Is plastic debris from repeated use a contamination concern in a medical environment?
- I think 1000 rotation
- Just the weight of the component
- Yes

And all parts in the design are made using 3D resin printing
 