I have ultrasonic data for a thick walled elbow that show the pipe wall thinning (due to errosion / corrosion) however the wall thickness is non-symetrical at various cross sections and is more pronounced in the turn of the elbow. From this data I can develop a 3-D model. I need to identify the maximum principal stresses in the elbow. I have access to ansys and abaqus but there is no basic model for this application in the library of either program. Does anyone know where I can obtain a base model for this application in ansys or abaqus or does anyone recommend another program for this application? Do I superimpose the thermal stress results with the hoop stress results? I have been required to use an FEA program to provide a look at the stress profile but should I pull out my Peng and Peng book and just look at the stresses where the wall thickness is a min?Thank you in advance for any help.
 

Take a look at API-579/ASME FFS-1. What you are trying to do is considered a "Level 3" analysis.

However, there is such a thing as a "Level 2" analysis which does not require the use of FEA, and is ananalytical approach you can do on a spreadsheet.

I'd start with a Level 2 analysis, and only perform Level 3 if it is necessary.

All the best.



 
Thanks Steve and Mr. Meyers for the lead. I really did not know where to start.

Gene
 
Mr. Steve or Mr. Meyers in the FFS-2 manual they reference a "MAT" - which is a design requirement temperature but it is never defined. Do you know what "MAT" refers to and how it is defined?

thanks
Gene
 
Check out paragraph 3.1.4.
 
TGS4 (Mechanical)

Thank you

Steve
 