MarkSRF

Materials
Joined
Aug 1, 2002
Messages
5
Location
US
If anyone has information on pgk grade tool steel it would be appreciated. We are looking to use it as a cutting tool primarily for our martensite. Any knowledge on its properties or in general would help. I have heard it may be a knife steel similar to vascowear but no specifics.
 