I want to know what type of pressure is the partial pressure of gas in Nitriding potential = (pNH3)/(pH2)^3/2.
I mean is it static, dynamic or total pressure.

Also how this pressure can be measured in a nitriding furnace for on line control of Nitriding potential.
Link to references will be appreciated.
 
The nitrogen potential is a function of temperature and the initial pressures of NH3 and any added H2. After the gases reach thermodynamic equilibrium at a temperature, the nitriding potential at the solid surface in equilibrium with the gas phase is given as:

KN = PNH3/PH23/2

--- H.J. Grabke, 'Kinerics of Gas-Solid Interactions,' Mater. Sci. Forum, Vol 154, p 69-85 (1994).

A recent, on-line article that may be useful: "Kinetics of Microstructure Evolution during Gaseous Thermochemical Surface Treatment" by Marcel A.J. Somers and Thomas Christiansen, Journal of Phase Equilibria and Diffusion, vol.26, pp. 520-528 (2005).

An article on controlling and measuring nitriding potential (same article, 2 links for luck):
Note: search the Industrial Heating (magazine) website for more info.

A vendor's process overview:
 