Aug 27, 2010 #1 ctowerh Mechanical Joined Mar 7, 2005 Messages 6 Location US Does anyone know of a good paint process for pad printing / hot stamping PETE that will hold up to dishwasher use?
Does anyone know of a good paint process for pad printing / hot stamping PETE that will hold up to dishwasher use?
Aug 31, 2010 #2 MikeHalloran Mechanical Joined Aug 29, 2003 Messages 14,450 Location US I'm guessing "no". How about using mold inserts to carry the information you would stamp if it were possible? Mike Halloran Pembroke Pines, FL, USA Upvote 0 Downvote
I'm guessing "no". How about using mold inserts to carry the information you would stamp if it were possible? Mike Halloran Pembroke Pines, FL, USA
Sep 1, 2010 #3 mcgyvr Mechanical Joined Aug 8, 2006 Messages 1,457 Location US I'd call tech support of a screen/pad printing ink company (we use Nazdar) they have some inks that will adhere to polyester/polyethylene... Upvote 0 Downvote
I'd call tech support of a screen/pad printing ink company (we use Nazdar) they have some inks that will adhere to polyester/polyethylene...
Sep 1, 2010 #4 Compositepro Chemical Joined Oct 22, 2003 Messages 7,841 Location US Corona treatment is often required just prior to printing on plastics. Upvote 0 Downvote