I'm new to the site and have read a tremendous amount of information so far (although I'm still learning to navigate the site)It is obvious that there are a lot of folks here with a lot of History and experience.
My question is as follows:
1.
Can you write a WPS for Carpenter 20 or Inconel from a PQR that was tested on Monel with-out further testing? "Just write it using the original variables with new base metal and filler wire"
This is without impact testing etc., ASME (no specialties in the PQR) OR can you just follow the Procedure Specification I already have for P-4X Monel,AL6XN etc.
I believe that the fillers have equivalent F-#'s and that the base metals are P-4X
Thanks
Tom
p.s. aside from studying AWS B2.1:2000, Is there any available sites etc. that are geared around this Topic?
My question is as follows:
1.
Can you write a WPS for Carpenter 20 or Inconel from a PQR that was tested on Monel with-out further testing? "Just write it using the original variables with new base metal and filler wire"
This is without impact testing etc., ASME (no specialties in the PQR) OR can you just follow the Procedure Specification I already have for P-4X Monel,AL6XN etc.
I believe that the fillers have equivalent F-#'s and that the base metals are P-4X
Thanks
Tom
p.s. aside from studying AWS B2.1:2000, Is there any available sites etc. that are geared around this Topic?