What would be the consequence of tightening A bolt beyound its recommended bolt load. The recommended operational bolt load is 430 kN and we are planning to tight the bolt via hydraulic bolt tensioner and approximately achieving more than 670 kN bolt load/bolt. 430kN bolt load is recommended by vendor of the equipment. The operational condition of the equipment is 140 kg/cm2 and 150 deg Celsius.

How far these recommended bolt loads are from yield point of bolt?
Specs of bolt: 2-1/2" UN8 B7 studs.
 
Last edited:
Min Yield strength of this bolt is 720 MPa, tensile is 860 MPa.
Tensile area is A= 645.16 mm2
Therefore Min yield load is 464.8 kN
Max load is 554.8 kN

So the recommended preload is 90% of yield strength.
If you preload to 670kN you will probably break it before reaching the load.

Hope it helps!
 
Additionally, at 150°C you're not going to have the mechanical properties at the same level as room temp.
 
Thank you for your response. I think the tensile area used here is quite small. the studs diameter is 63.5 from which calculated tensile area should be 3165 mm2. using that min yield load is around 2000 kN.
 
You are right, I miss copied the value in excel. The tensile area is 2854 mm2 ( a bit lower than you said due to the threads etc).

Yield 2054 kN
Tensile 2454 kN

Then if you preload 670 kN should be alright is around 30% yield.

You're in the spec service temperature range -100˚C to 565˚C so it should be alright.

check this specs also :) it's in imperial units.
1750845292674.png
 
This spec sheet is really helpful. Can you please share its reference. And where are the spec service temps range and bolt material is mentioned?
 