Hello all...
I have a dead stock of molecular sieve. It's been in my logistic warehouse since maybe 15 or 20 years ago, and i'm looking for any possibilities that i can still use it.
It is a 13X type molecular sieve with 1/16" pelleted grain size. I will using it for an absorption of H2O and CO2 and any hidrocarbon in air pretreatment before entering coldbox of N2 plant
What is the parameter for determining that the molecular sieve is still in good condition?
What kind of analysis that my laboratorium should run to that molsieve?
What is the ideal run time for a molecular sieve in operation since my N2 plant have never change its molsieve since 15 years? And what is the parameter for changing molsieve decision?
thanks before for your response
Devax Rayz,
Junior Process Engineer
I have a dead stock of molecular sieve. It's been in my logistic warehouse since maybe 15 or 20 years ago, and i'm looking for any possibilities that i can still use it.
It is a 13X type molecular sieve with 1/16" pelleted grain size. I will using it for an absorption of H2O and CO2 and any hidrocarbon in air pretreatment before entering coldbox of N2 plant
What is the parameter for determining that the molecular sieve is still in good condition?
What kind of analysis that my laboratorium should run to that molsieve?
What is the ideal run time for a molecular sieve in operation since my N2 plant have never change its molsieve since 15 years? And what is the parameter for changing molsieve decision?
thanks before for your response
Devax Rayz,
Junior Process Engineer