I have a very old column ( from the sixties) in which some shells and one head are in A-265.
The remaining is in A-285 Gr. C
Cladis S.S. over the whole colomn (inside)
design code is ASME VIII div.1.
Column is at 3.5 bag and 375 Celsius
I have to re-assess this column (chapter 4 and 5 of API 597)
My question is what is this A-265 ??
It looks like an obsolete ASTM material !!
How does it compares with A 285 Gr. C ??
What is its allowable stress say at 200, 300 , 370 degree Celsius.
Any idea, tips...Thanks
The remaining is in A-285 Gr. C
Cladis S.S. over the whole colomn (inside)
design code is ASME VIII div.1.
Column is at 3.5 bag and 375 Celsius
I have to re-assess this column (chapter 4 and 5 of API 597)
My question is what is this A-265 ??
It looks like an obsolete ASTM material !!
How does it compares with A 285 Gr. C ??
What is its allowable stress say at 200, 300 , 370 degree Celsius.
Any idea, tips...Thanks