I am working on ASME B&PV Section VIII, Div. 1 calcs for an existing ASME "U" stamped vessel at my facility. The problem is that while the vessel nozzles meet the minimum thickness requirements per UG-27, they do not meet the thickness requirements of UG-45. The nozzles range from 1" to 3" Schedule 5 pipe. The vessel was built in 1991 to the 1986 edition of the Code. I couldn't find the 1986 edition of the Code to see if the UG-45 requirement existed. But the 1989 edition did have it.
My question is how could this vessel be Code stamped if it did not meet UG-45? Does anyone any suggestions how I can keep using this as a Code vessel without derating it? Would ASME Code allow a finite element analysis instead?
Thanks!
My question is how could this vessel be Code stamped if it did not meet UG-45? Does anyone any suggestions how I can keep using this as a Code vessel without derating it? Would ASME Code allow a finite element analysis instead?