We believe if we have a nozzle > NPS 10" or > 1 1/8" thickness, we need to use the joint efficiency from UW-12 on the long weld seam of the nozzle in addition to the weld factor in the allowable stress from Section II.
The question is how does whether you spot x-ray the vessel section Category B or C joints affect the nozzle efficiency per UW-11 (a) (5) (b)?
Appendix L-9.2.4 seems to indicate this has a factor on when you "double dip" and take the weld efficiency in addtion to the welded stress value from Section II.
 
Replies continue below

Recommended for you

Jordan123,

If this is welded pipe with no Category B or C butt welds, the requirements of UW-11(a)(5)(b) do not apply and you could use E = 1 as directed by UW-12(e) and UW-12(d) for your UG-27(c)(1) calculations.

If this a rolled plate nozzle the joint efficiency would be from Table UW-12 for Type 1 or Type 2 butt joints and extent of RT.

The exception is when performing area replacement calculations in accordance with UG-37; in which case joint efficiency is always E = 1 for trn.

You can reference Interpretation VIII-1-01-89.