What is the maximum amount of N that can be tolerated in CA6NM?
Apart from possible porosity problems due to the solubility, N is an austenite stabilisor. I expect the more nitrogen, the more retained austenite. From what percentage is this becoming a problem?
A close match to CA6NM: DIN/SEW X4CrNi13.4, 1.4313 even specifies a minimum of 0.02% N, but doesn't state a maximum.
Thanks for any help on this subject,
Apart from possible porosity problems due to the solubility, N is an austenite stabilisor. I expect the more nitrogen, the more retained austenite. From what percentage is this becoming a problem?
A close match to CA6NM: DIN/SEW X4CrNi13.4, 1.4313 even specifies a minimum of 0.02% N, but doesn't state a maximum.