Aug 2, 2006 #1 3lilaggies Mechanical Joined May 4, 2006 Messages 52 Location US Can I write a new WPS with no PWHT using an old PQR with PWHT? Using ASME section 8 and 9, any code reference or guidance would be helpful.
Can I write a new WPS with no PWHT using an old PQR with PWHT? Using ASME section 8 and 9, any code reference or guidance would be helpful.
Aug 2, 2006 #2 weldtek Materials Joined Feb 12, 2005 Messages 897 Location US No. Refer to Sec IX for the applicable process, then look at QW 407. Upvote 0 Downvote
Aug 2, 2006 Thread starter #3 3lilaggies Mechanical Joined May 4, 2006 Messages 52 Location US Right I found it PWHT is an essential variable. I needed to read one page further. HaHaHa. Thanks for the help Upvote 0 Downvote