We have a pressure Vessel ID 5,029mm X 12,920mm OAL x 24/20mm Thk – SA 516 Gr.60N + HIC, Originally Designed as per Div 1 with MDMT of -2 Deg C, U stamped.
There is a Process Requirement to Revise the MDMT to -29 Deg C.
For the new MDMT, the vessel need to be "R" Stamped.
We have the following documents.
1. MTCs of all Shell / Dished End Plates, having Different Heat Nos, all Impact Tested at -46 Deg C (at colder temp than required MDMT of -29 Deg C)
2. PQRs for all pressure parts welding have been Impact Tested at - 29 Deg C.
With the above documents (1 and 2), can we approach ASME Inspector for "R" Stamp?
Is it Mandatory that all the Welding Consumables (Pressure parts welding)impact Tested at -29 Deg C or Colder? (The QC Dossier with us, does not included MTCs for the Welding Consumables)..
Need an expert advise
Regards
There is a Process Requirement to Revise the MDMT to -29 Deg C.
For the new MDMT, the vessel need to be "R" Stamped.
We have the following documents.
1. MTCs of all Shell / Dished End Plates, having Different Heat Nos, all Impact Tested at -46 Deg C (at colder temp than required MDMT of -29 Deg C)
2. PQRs for all pressure parts welding have been Impact Tested at - 29 Deg C.
With the above documents (1 and 2), can we approach ASME Inspector for "R" Stamp?
Is it Mandatory that all the Welding Consumables (Pressure parts welding)impact Tested at -29 Deg C or Colder? (The QC Dossier with us, does not included MTCs for the Welding Consumables)..
Need an expert advise