We have a pressure Vessel ID 5,029mm X 12,920mm OAL x 24/20mm Thk – SA 516 Gr.60N + HIC, Originally Designed as per Div 1 with MDMT of -2 Deg C, U stamped.
There is a Process Requirement to Revise the MDMT to -29 Deg C.

For the new MDMT, the vessel need to be "R" Stamped.

We have the following documents.
1. MTCs of all Shell / Dished End Plates, having Different Heat Nos, all Impact Tested at -46 Deg C (at colder temp than required MDMT of -29 Deg C)
2. PQRs for all pressure parts welding have been Impact Tested at - 29 Deg C.

With the above documents (1 and 2), can we approach ASME Inspector for "R" Stamp?
Is it Mandatory that all the Welding Consumables (Pressure parts welding)impact Tested at -29 Deg C or Colder? (The QC Dossier with us, does not included MTCs for the Welding Consumables)..

Need an expert advise

Regards

 
Replies continue below

Recommended for you

My expert advise is to review the National Board Inspection Code (NBIC), Part 3 for the rules to follow for an alteration. This will require an organization in possession of a valid National Board R-Certificate to perform Repairs and Alterations. The organization will have an Inspector who has an R endorsement. It is not an ASME Inspector.

The reduction in MDMT is an alteration. Your other option is to review API 510 for alterations to pressure vessels.
 